MetaTOC stay on top of your field, easily

Microstructure-controlled corrosion in directed energy deposited Ni-based superalloy: A review

, , ,

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering

Published online on

Abstract

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, Ahead of Print.
Nickel-based superalloy Inconel 718 is widely used in aerospace, marine, and energy sectors owing to its exceptional high-temperature strength, creep resistance, and corrosion performance. However, conventional manufacturing routes suffer from long lead ...