Maintenance-Triggered cascade failure in a marine diesel engine: Fractographic and numerical analysis of connecting rod rupture caused by valve lash deviation
Published online on April 19, 2026
Abstract
Proceedings of the Institution of Mechanical Engineers, Part M: Journal of Engineering for the Maritime Environment, Ahead of Print.
Fracture of the connecting rod in marine diesel engines results in catastrophic mechanical failure, immediate loss of propulsion, and extensive internal damage. While fatigue and overload are often cited, the role of maintenance deviation remains ...
Fracture of the connecting rod in marine diesel engines results in catastrophic mechanical failure, immediate loss of propulsion, and extensive internal damage. While fatigue and overload are often cited, the role of maintenance deviation remains ...