MetaTOC stay on top of your field, easily

Investigation of high temperature tensile properties of TLP bonded IN 718 superalloy

, , ,

Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications

Published online on

Abstract

Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications, Volume 240, Issue 5, Page 860-880, May 2026.
The joining of Inconel 718 superalloy was achieved by transient liquid phase (TLP) bonding and utilising a BNi-2 interlayer material. The microstructural changes and high-temperature tensile behaviour of IN 718 joints were investigated in detail. The ...