Influence of heat input on the microstructures, mechanical properties, and corrosion behaviour of dissimilar Nimonic 75 superalloy and Nitronic 50 austenitic stainless steel GTA welds

, , , ,

Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications

Published online on

Abstract

Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications, Ahead of Print.
The dissimilar weldments of Nimonic 75 superalloy and Nitronic 50 austenitic stainless steel (ASS) are of great importance for high-temperature structural applications where cost-effectiveness and performance are critical. In this study, dissimilar ...