MetaTOC stay on top of your field, easily

Optimization of wire electrical discharge machining process parameters on Inconel 690 superalloy via Taguchi technique

, , ,

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering

Published online on

Abstract

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, Volume 240, Issue 3, Page 3346-3353, June 2026.
The research work deals with the improvement of wire electrical discharge machining process parameters for Inconel 690 super alloy. The goal of optimization is to achieve a maximum material removal rate (MRR) and a minimum surface roughness (SR). Brass ...