MetaTOC stay on top of your field, easily

Effect of heat treatment on the morphology and mechanical properties of the novel Ni-based superalloy with machinability assessment through electrical discharge machining

, ,

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering

Published online on

Abstract

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, Ahead of Print.
A superalloy is a high-performance alloy used for achieving stability and strength at elevated temperatures. The present work aims at investigating heat treatment characteristics of a single crystal Nickel-based superalloy used in aero turbine blades in ...