Prediction of white layer thickness with machining time in milling of nickel-based superalloy Inconel 718 considering time-varying tool wear and tool temperature effect
Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture
Published online on October 16, 2025
Abstract
Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, Ahead of Print.
White layer has a significant impact on the surface quality of workpieces, so the accurate prediction of white layer thickness (WLT) is crucial. However, the present prediction models ignore the situation that WLT changes with machining time due to time-...