Surface analysis of prepared nanotungsten oxide and effect on the physical, mechanical, and radiation shielding properties of composites based on nitrile butadiene rubber and agro-waste bean fibers

, , , , , , , , ,

Journal of Composite Materials

Published online on

Abstract

Journal of Composite Materials, Ahead of Print.
This study addresses the growing demand for efficient, versatile, and non-toxic radiation shields by developing a sustainable nanocomposite using waste bean fiber as a bio-based framework. A nitrile butadiene rubber (NBR) nanocomposite was prepared, ...